Mix ratios · Mortar types (ASTM C270)
Mortar types (ASTM C270)
Type O mortar
A low-strength mortar (min 350 psi) for interior non-load-bearing walls and for re-pointing soft historic brick where a hard mortar would cause damage.
Proportions & strength
Planning reference. Strengths are typical values for a well-made mix at 28 days, not a guaranteed design strength. Structural work must follow your local building code and a qualified engineer's mix design.
Where Type O is used
A low-strength mortar (min 350 psi) for interior non-load-bearing walls and for re-pointing soft historic brick where a hard mortar would cause damage.
Mortar type matters more than most people expect: a mortar much stronger than the units it beds will transfer movement into the masonry and spall the faces. Pick the weakest mortar that meets the structural and exposure demand.
Need quantities? The volume calculators give the cubic yards, cubic metres and bag counts for the pour this mix goes into.
Applications
Jobs that use Type O
Same family
Other mortar types (astm c270)