Masonry grout

Coarse masonry grout

Adds pea gravel for larger grout spaces (bond beams, wide cores). Still placed at a high slump so it consolidates fully around reinforcement.

Mix ratio
1 : 3 : 2
Cement : Sand : Pea gravel

Proportions & strength

DesignationCoarse grout
Ratio (by volume)1 : 3 : 2
Cement1 part
Sand3 parts
Pea gravel2 parts
Typical compressive strength2,000 psi · 14 MPa
Typical useFilling wider block cores and bond beams.
Planning reference. Strengths are typical values for a well-made mix at 28 days, not a guaranteed design strength. Structural work must follow your local building code and a qualified engineer's mix design.

Where Coarse grout is used

Adds pea gravel for larger grout spaces (bond beams, wide cores). Still placed at a high slump so it consolidates fully around reinforcement.

Grout is placed at a high slump so it flows fully around reinforcement and fills the cavity without voids. It is not the same as mortar, and it is not the same as tile grout.

Need quantities? The volume calculators give the cubic yards, cubic metres and bag counts for the pour this mix goes into.

Applications